Inconel 601 apaļā stieņa standarta izmēri

Diametrs vai
Platums
(mm)
Svars uz metru Sekciju apgabals Perimetrs
  Kvadrāts
(kg)
Apaļš
(kg)
Kvadrāts
(cm²)
Apaļš
(cm²)
Kvadrāts
(cm)
Apaļš
(cm)
5.0 0.20 0.15 0.25 0.20 2.0 1.57
5.5 0.24 0.19 0.30 0.24 2.2 1.78
6.0 0.28 0.22 0.36 0.28 2.4 1.88
7.0 0.38 0.30 0.49 0.38 2.8 2.20
8.0 0.50 0.39 0.64 0.50 3.2 2.51
9.0 0.64 0.50 0.81 0.64 3.6 2.83
10 0.73 0.63 1.00 0.79 4.0 3.14
11 0.95 0.75 1.21 0.95 4.4 3.46
12 1.13 0.89 1.44 1.13 4.8 3.77
14 1.54 1.21 1.96 1.54 5.6 4.40
16 2.01 1.58 2.56 2.01 6.4 5.03
18 2.54 2.00 3.24 2.54 7.2 5.65
20 3.14 2.47 4.00 3.14 8.0 6.28
22 3.80 2.98 4.84 3.80 8.8 6.91
25 4.91 3.85 6.25 4.91 10.0 7.85
28 6.15 4.83 7.84 6.16 11.2 8.80
32 8.04 6.31 10.24 8.04 12.8 10.05
36 10.17 7.99 12.96 10.18 14.4 11.31
40 12.56 9.86 16.00 12.57 16.0 12.57
45 15.90 12.49 20.25 15.90 18.0 14.14
50 19.62 15.41 25.00 19.64 20.0 15.71
56 24.62 19.34 31.36 24.63 22.4 17.59
63 31.16 24.47 36.69 31.17 25.2 19.79
71 39.57 31.08 50.41 39.59 28.4 22.31
80 50.24 39.46 64.00 50.27 32.0 25.13

 

Inconel UNS N06601 Bright Round Bar tolerance

Inconel 601 apaļā stieņa pielaide ISO "H" sērija MM
Izmērs (mm) H12 H11 H10 H9 H8 H7 H6 H5
Vairāk nekā 180 - 250 +0.46/0 +0.29/0 +0.185/0 +0.115/0 +0.072/0 +0.046/0 +0.029/0 +0.02/0
Vairāk nekā 120 - 180 +0.4/0 +0.25/0 +0.16/0 +0.1/0 +0.063/0 +0.04/0 +0.025/0 +0.018/0
Vairāk nekā 80 - 120 +0.35/0 +0.22/0 +0.14/0 +0.087/0 +0.054/0 +0.035/0 +0.022/0 +0.015/0
Vairāk nekā 50 - 80 +0.3/0 +0.19/0 +0.12/0 +0.074/0 +0.046/0 +0.03/0 +0.019/0 +0.013/0
Vairāk nekā 30 - 50 +0.25/0 +0.16/0 +0.1/0 +0.062/0 +0.039/0 +0.025/0 +0.016/0 +0.011/0
Vairāk nekā 18 - 30 +0.21/0 +0.13/0 +0.084/0 +0.052/0 +0.033/0 +0.021/0 +0.013/0 +0.009/0
Vairāk nekā 10 - 18 +0.18/0 +0.11/0 +0.07/0 +0.043/0 +0.027/0 +0.018/0 +0.011/0 +0.008/0
Vairāk nekā 6 - 10 +0.15/0 +0.09/0 +0.058/0 +0.036/0 +0.022/0 +0.015/0 +0.009/0 +0.006/0
Vairāk nekā 3 - 6 +0.12/0 +0.075/0 +0.048/0 +0.03/0 +0.018/0 +0.012/0 +0.008/0 +0.005/0
~ līdz 3 +0.1/0 +0.06/0 +0.04/0 +0.025/0 +0.014/0 +0.01/0 +0.006/0 +0.004/0

 